Flow stress analysis and Arrhenius constitutive equation of near β titanium alloy Ti-55511 during thermoplastic deformation
LUO Deng1, HU Bin2, WANG Zhen1, ZHOU Wenhao1, KONG Bin3, ZHANG Xiaoyong2
1. Xiangtan Iron & Steel Group Co., Ltd., Xiangtan 411100, China; 2. State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083, China; 3. Hunan Xiangtou Goldsky Titanium Metal Co., Ltd., Changsha 410205, China
Abstract:Hot deformation behavior of Ti-55511 titanium alloy was studied at deformation temperatures of 700-850 ℃, strain rates of 0.01-10 s-1 and true strain of 0.6. The results indicate that the flow behavior of Ti-55511 titanium alloy is significantly affected by deformation temperature and strain rate. With the decrease of temperature and the increase of strain rate, the peak stress increases. In order to eliminate the deformation temperature rise effect in the process of hot compression and improve the accuracy of the model, a new temperature correction method was adopted in this paper. The temperature correction of the experimental flow stress curve was carried out through the Arrhenius constitutive equation derivation and combined with the mathematical extrapolation method. The results show that with the decrease of deformation temperature and the increase of strain rate, temperature rise and flow stress increment increase. The Arrhenius constitutive equation of strain-compensated is established, and the value of correlation coefficient (R2) and average absolute relative error (AARE) between experimental and predicted stress are 0.991 and 6.65%, respectively. This indicates that the established constitutive equation can accurately predict the flow stress under different thermal deformation conditions.
罗登, 胡斌, 王振, 周文浩, 孔玢, 张晓泳. 近β钛合金Ti-55511热塑性变形的流变应力分析与Arrhenius本构方程研究[J]. 粉末冶金材料科学与工程, 2023, 28(3): 212-222.
LUO Deng, HU Bin, WANG Zhen, ZHOU Wenhao, KONG Bin, ZHANG Xiaoyong. Flow stress analysis and Arrhenius constitutive equation of near β titanium alloy Ti-55511 during thermoplastic deformation. Materials Science and Engineering of Powder Metallurgy, 2023, 28(3): 212-222.
[1] LI C M, HUANG L, LI C L, et al.Research progress on hot deformation behavior of high-strength β titanium alloy: flow behavior and constitutive model[J]. Rare Metals, 2022, 41(5): 1434-1455. [2] CHEN W, LI C, ZHANG X Y, et al.Deformation-induced variations in microstructure evolution and mechanical properties of bi-modal Ti-55511 titanium alloy[J]. Journal of Alloys and Compounds, 2019, 783: 709-717. [3] 熊智豪, 李志尚, 杨平, 等. 大规格TC18钛合金棒材多火次锻造中β相织构演变规律[J]. 钛工业进展, 2021, 38(6): 6-11. XIONG Zhihao, LI Zhishang, YANG Ping, et al.Evolution of β phase texture of large size TC18 titanium alloy bar during multi-pass forging[J]. Titanium Industry Progress, 2021, 38(6): 6-11. [4] SU L P, LIU H Y, JING L, et al.Flow stress characteristics and microstructure evolution during hot compression of Nb-47Ti alloy[J]. Journal of Alloys and Compounds, 2019, 797: 735-743. [5] YIN Z K, SUN Z H, HUANG L, et al.Feasibility analysis of obtaining tri-modal microstructure by multi-pass conventional forging combined with dual heat treatment for near-α titanium alloy with different initial microstructures[J]. International Journal of Lightweight Materials and Manufacture, 2023, 6(1): 25-32. [6] 黄朝文, 赵永庆, 辛社伟, 等. 高强韧钛合金热加工变形特征及其影响因素[J]. 钛工业进展, 2016, 33(1): 8-14. HUANG Chaowen, ZHAO Yongqing, XIN Shewei, et al.Hot deformation characteristics of high strength-toughness titanium alloys and its influencing factors[J]. Titanium Industry Progress, 2016, 33(1): 8-14. [7] 刘彬, 曾凡沛, 卢金忠, 等. 粉末冶金纯钛的热变形本构方程及热加工图研究[J]. 粉末冶金材料科学与工程, 2015, 20(4): 499-504. LIU Bin, ZENG Fanpei, LU Jinzhong, et al.Constitutive equation and thermal processing map of powder metallurgy pure titanium[J]. Materials Science and Engineering of Powder Metallurgy, 2015, 20(4): 499-504. [8] 王琪, 文智, 王斌, 等. 粉末冶金TA15钛合金的高温塑性变形行为[J]. 粉末冶金材料科学与工程, 2013, 18(5): 647-654. WANG Qi, WEN Zhi, WANG Bin, et al.High temperature plastic deformation behavior of powder metallurgic TA15 titanium alloy[J]. Materials Science and Engineering of Powder Metallurgy, 2013, 18(5): 647-654. [9] CHEN Y, LI J S, TANG B, et al.Texture evolution and dynamic recrystallization in a beta titanium alloy during hot-rolling process[J]. Journal of Alloys and Compounds, 2015, 618: 146-152. [10] YU J X, LI Z J, QIAN C, et al.Investigation of deformation behavior, microstructure evolution, and hot processing map of a new near-α Ti alloy[J]. Journal of Materials Research and Technology, 2023, 23: 2275-2287. [11] ZHAO T L, ZHANG B, ZHANG Z J, et al.Deformation behavior and microstructural evolution of pure Ti produced by hot compressing[J]. Journal of Materials Research and Technology, 2022, 21: 2383-2399. [12] 冯秋元, 郭佳林, 杨军, 等. Ti60高温钛合金的热变形行为Ⅰ: 本构方程[J]. 塑性工程学报, 2021, 28(11): 158-166. FENG Qiuyuan, GUO Jialin, YANG Jun, et al.Hot deformation behavior of Ti60 high temperature titanium alloy I: constitutive equations[J]. Journal of Plasticity Engineering, 2021, 28(11): 158-166. [13] LIU J L, ZENG W D, LAI Y J, et al.Constitutive model of Ti17 titanium alloy with lamellar-type initial microstructure during hot deformation based on orthogonal analysis[J]. Materials Science and Engineering A, 2014, 597: 387-394. [14] RAN C, SHENG Z M, CHEN P W, et al.Effect of microstructure on the mechanical properties of Ti-5Al-5Mo- 5V-1Cr-1Fe alloy[J]. Materials Science and Engineering A, 2020, 773: 138728. [15] YANG H B, BU H Y, LI M N, et al.Prediction of flow stress of annealed 7075 Al alloy in hot deformation using strain-compensated Arrhenius and neural network models[J]. Materials, 2021, 14(20): 5986. [16] 彭嘉豪, 孙前江, 周建伟,等. TC4-DT钛合金高温热变形及加工图[J]. 中国有色金属学报, 2022, 32(4): 994-1003. PENG Jiahao, SUN Qianjiang, ZHOU Jianwei, et al.High temperature thermal deformation and processing of TC4-DT titanium alloy[J]. The Chinese Journal of Nonferrous Metals, 2022, 32(4): 994-1003. [17] 周亚利, 杨秋月, 张文玮, 等. 具有层片状α相组织的TB8钛合金热变形行为及本构方程[J]. 材料工程, 2021, 49(1): 75-81. ZHOU Yali, YANG Qiuyue, ZHANG Wenwei, et al.Hot deformation behavior and constitutive equation of TB8 titanium alloy with a lamellar structure of α phase[J]. Journal of Materials Engineering, 2021, 49(1): 75-81. [18] SHI S X, GE J Y, LIN Y C, et al.High-temperature deformation behavior and recrystallization mechanism of a near beta titanium alloy Ti-55511 in β phase region[J]. Materials Science and Engineering A, 2022, 847: 143335. [19] ZHAO J, ZHONG J, YAN F, et al.Deformation behaviour and mechanisms during hot compression at supertransus temperatures in Ti-10V-2Fe-3Al[J]. Journal of Alloys and Compounds, 2017, 710: 616-627. [20] 朱鸿昌. TB17钛合金热加工过程组织演变规律研究[D]. 南昌: 南昌航空大学, 2019. ZHU Hongchang.Study on microstructure evolution of TB17 titanium alloy during hot working process[D]. Nanchang: Nanchang Hangkong University, 2019. [21] LI L, ZHOU J, DUSZCZYK J, et al.Determination of a constitutive relationship for AZ31B magnesium alloy and validation through comparison between simulated and real extrusion[J]. Journal of Materials Processing Technology, 2006, 172(3): 372-380. [22] 尚丽梅, 王春旭, 韩顺, 等. 基于摩擦-温度双修正的Maraging250钢热变形行为及热加工图[J]. 金属热处理, 2021, 46(5): 111-117. SHANG Limei, WANG Chunxu, HAN Shun, et al.Hot deformation behavior and processing maps of Maraging250 steel based on friction and temperature double correction[J]. Heat Treatment of Metals, 2021, 46(5): 111-117. [23] GOETZ R L, SEMIATIN S L.The adiabatic correction factor for deformation heating during the uniaxial compression test[J]. Journal of Materials Engineering and Performance, 2001, 10(6): 710-717. [24] DADRAS P, THOMAS JR J F. Characterization and modeling for forging deformation of Ti-6Al-2Sn-4Zr- 2Mo-0.1Si[J]. Metallurgical Transactions A: Physical Metallurgy and Materials Science, 1981, 12A:1867-1876. [25] LI C M, HUANG L, ZHAO M J, et al.Characterization of hot workability of Ti-6Cr-5Mo-5V-4Al alloy based on hot processing map and microstructure evolution[J]. Journal of Alloys and Compounds, 2022, 905: 164161. [26] REZAEI ASHTIANI H R, SHAHSAVARI P. Constitutive modeling of flow behavior of precipitation-hardened AA7022-T6 aluminum alloy at elevated temperature[J]. Journal of Alloys and Compounds, 2020, 30(11): 2927-2940.